Our site saves small pieces of text information (cookies) on your device in order to deliver better content and for statistical purposes. You can disable the usage of cookies by changing the settings of your browser. By browsing our site without changing the browser settings you grant us permission to store that information on your device.

A new scintillator Nd3+ doped LaBr3

X. GAO1, Y. J. HE1,* , Y. B. CHEN1

Affiliation

  1. Department of Physics, Tsinghua University, Beijing 10084, P. R. China

Abstract

Nd3+ doped single crystals, LaBr3:1.25% Nd 3+3+, LaBr3 :2.5% Nd3+3+, LaBr3 :5% Nd3+ and LaBr3 :10% Nd3+3+, were grown by vertical Bridgman process. The scintillation properties including light output, ene rgy resolution, time profile, energy proportionality of the single crystals and the luminescence of polycrystalline power were measured. 2.5% Nd3+ doped LaBr 3 exhibited the best scintillation properties while other doped ones weren’ t so transparent after polished.

Keywords

Scintillation, Scintillator, Luminescence, LaBr3:Nd 3+.

Citation

X. GAO, Y. J. HE, Y. B. CHEN, A new scintillator Nd3+ doped LaBr3, Optoelectronics and Advanced Materials - Rapid Communications, 5, 4, April 2011, pp.341-343 (2011).

Submitted at: March 25, 2011