Abstract
Polyethylene glycol was added in the sol gel precursor to prepare porous cerium titanate. The cerium titanate samples are
composed of brannerite structured CeTi2O6 of monoclinic system and a small proportion of cubic CeO2. FT infrared and
FT Far infrared spe ctra demonstrate the surface adsorbed water molecules and metal oxide bonds in the materials. The BET
specific surface areas of the nonporous and porous cerium titanates are 1.7 and 16.2 m2/g, and the pore volume of these two
samples are 0.0036 and 0.0232 cm3/g, respectively. The chemical shift of oxygen and titanium atoms in the porous cerium
titanate is not found after using PEG4000. The first order reaction rate constant for photocatalytic degradation of ofloxacin on
the nonporous sample is 1.340×10 2 min1, while it is as high as 6.852×10 2 min1 on the porous cerium titanate..
Keywords
Cerium Titanate Photocatalysis PEG4000, Ofloxacin Degradation.