Abstract
Di-calcium phosphate dihydrate triclinic CaHPO4.2H2O was heated at 750 oC and 450 oC to obtain the tetragonal β-Ca2P2O7 and grey-coloured tetragonal γ-Ca2P2O7 phase. The pellets of β-Ca2P2O7 γ-Ca2P2O7 were prepared and dried at 120 oC for 4 hours. The pellets having mean thickness of 2 mm were characterized by XRD, optical microscopy, FTIR, TGA, SEM, UV-visible spectroscopy and dc-electrical measurements. Before sintering micro-cracks were seen however these cracks were disappeared after sintering at 750 oC. XRD confirmed the single crystalline phase. UV-vis. Spectra showed absorption in UV-region. DC-electrical resistivity exhibited that β-Ca2P2O7 is more conducting as compared to γ-Ca2P2O7 phase..
Keywords
CaHPO4.2H2O, β-Ca2P2O7 phase, γ-Ca2P2O7 phase, DC-electrical resistivity, XRD, FTIR.
Citation
IMTIAZ U. KHAWAJA, QURSHIA CHOUDHRY, ASIF MAHMOOD, ZAHEER ABAS GILANI, SHAUKAT ALI SHAHID, MUHAMMAD FAROOQ, Structural, morphological and electrical properties of heat treated CaHPO4 biomaterials, Optoelectronics and Advanced Materials - Rapid Communications, 9, 9-10, September-October 2015, pp.1171-1175 (2015).
Submitted at: July 7, 2015
Accepted at: Sept. 9, 2015