Our site saves small pieces of text information (cookies) on your device in order to deliver better content and for statistical purposes. You can disable the usage of cookies by changing the settings of your browser. By browsing our site without changing the browser settings you grant us permission to store that information on your device.

Uniform CaWO4:Ln (Ln = Eu3+, Dy3+) phosphors: solvothermal synthesis and luminescent properties

W. WANG1, W. PAN2, Y. DAI1, S. GAI1, P. YANG1,*

Affiliation

  1. College of Material Science and Chemical Engineering, Harbin Engineering University, Harbin 150001, P. R. China
  2. College of Chemical Engineering and Food, Zhongzhou University , Zhengzhou 450044, China

Abstract

Uniform CaWO4:Ln (Ln = Eu3+, Dy3+) phosphors were successfully synthesized via the micro-emulsion mediated solvothermal process. The as-synthesized samples were well characterized by XRD, FESEM, TEM, XPS, photoluminescence (PL) spectra, and the kinetic decays, respectively. It is found that the as-synthesized phosphors are of high crystallinity and purity with regular octahedral morphology. Upon excitation by ultraviolet radiation, the CaWO4:Eu3+ phosphors show the characteristic 5D0– 7F1-4 emission lines of Eu3+, while the CaWO4:Dy3+ exhibits the characteristic 4F9/2–6H13/2–15/2 emission lines of Dy3+. It should be noted the PL intensities of the phosphors can be tuned by altering the doping concentration of Eu3+ and Dy3+..

Keywords

Solvothermal method, Luminescence, CaWO4, Microemulsion.